Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model

11.8K Views

11:10 min

May 23rd, 2018

DOI :

10.3791/57103-v

May 23rd, 2018


Przeglądaj więcej filmów

Atomic Layer Deposition

Rozdziały w tym wideo

0:04

Title

0:56

Atomic Layer Deposition (ALD) of Amorphous Vanadium Dioxide (VO2 ) on Sapphire Substrates

3:06

Annealing Amorphous VO2 Thin Films

4:45

Characterization of VO2 Films by Raman Spectroscopy

5:43

Characterization of VO2 Films by X-Ray Photoelectron Spectroscopy (XPS)

7:31

Morphological Characterization by Atomic Force Microscopy (AFM)

9:06

Results: Characterization of Amorphousand Crystalline VO2 Films

10:49

Conclusion

Powiązane Filmy

article

08:25

Chemical Vapor Deposition of an Organic Magnet, Vanadium Tetracyanoethylene

11.4K Views

article

10:52

Formation of Thick Dense Yttrium Iron Garnet Films Using Aerosol Deposition

9.2K Views

article

08:14

Improved Heterojunction Quality in Cu2O-based Solar Cells Through the Optimization of Atmospheric Pressure Spatial Atomic Layer Deposited
Zn1-xMgxO

12.1K Views

article

08:18

Synthesis and Characterization of High c-axis ZnO Thin Film by Plasma Enhanced Chemical Vapor Deposition System and its UV Photodetector Application

15.2K Views

article

08:58

Seedless Growth of Bismuth Nanowire Array via Vacuum Thermal Evaporation

8.3K Views

article

06:39

Aerosol-assisted Chemical Vapor Deposition of Metal Oxide Structures: Zinc Oxide Rods

13.0K Views

article

11:54

Growth and Electrostatic/chemical Properties of Metal/LaAlO3/SrTiO3 Heterostructures

10.2K Views

article

09:12

Production of Single Tracks of Ti-6Al-4V by Directed Energy Deposition to Determine the Layer Thickness for Multilayer Deposition

9.2K Views

article

09:41

Bulk and Thin Film Synthesis of Compositionally Variant Entropy-stabilized Oxides

9.4K Views

article

08:23

Niobium Oxide Films Deposited by Reactive Sputtering: Effect of Oxygen Flow Rate

7.3K Views

JoVE Logo

Prywatność

Warunki Korzystania

Zasady

Badania

Edukacja

O JoVE

Copyright © 2025 MyJoVE Corporation. Wszelkie prawa zastrzeżone