Growth and Electrostatic/chemical Properties of Metal/LaAlO3/SrTiO3 Heterostructures
Diogo Castro Vaz 1, Edouard Lesne 1,2, Anke Sander 1, Hiroshi Naganuma 1,3, Eric Jacquet 1, Jacobo Santamaria 1,4, Agnès Barthélémy 1, Manuel Bibes 1
1Unité Mixte de Physique CNRS/Thales, Université Paris-Saclay, 2Max Planck Institut für Mikrostrukturphysik, 3Department of Applied Physics, Tohoku University, 4Instituto de Magnetismo Aplicado, Universidad Complutense de Madrid

We fabricate metal/LaAlO3/SrTiO3 heterostructures using a combination of pulsed laser deposition and in situ magnetron sputtering. Through magnetotransport and in situ X-ray photoelectron spectroscopy experiments, we investigate the interplay between electrostatic and chemical phenomena of the quasi two-dimensional electron gas formed in this system.

JoVE Logo

Riservatezza

Condizioni di utilizzo

Politiche

Ricerca

Didattica

CHI SIAMO

Copyright © 2025 MyJoVE Corporation. Tutti i diritti riservati