Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition

12.3K Views

09:45 min

July 26th, 2016

DOI :

10.3791/54268-v

July 26th, 2016


Explore More Videos

Epitaxial Growth

Chapters in this video

0:05

Title

1:20

Cleaning the Germanium Substrate

2:46

Loading to the Vacuum System and Germanium Deoxidization

4:30

Thin Film ALD Growth and Annealing of the Strontium Titanate (STO) Film

7:23

Results: RHEED and X-ray Diffraction Analysis

8:41

Conclusion

Related Videos

article

08:45

Fabrication of Spatially Confined Complex Oxides

9.5K Views

article

08:49

Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films

14.2K Views

article

08:30

Monovalent Cation Doping of CH3NH3PbI3 for Efficient Perovskite Solar Cells

16.6K Views

article

11:54

Growth and Electrostatic/chemical Properties of Metal/LaAlO3/SrTiO3 Heterostructures

10.2K Views

article

08:00

Chemical Synthesis of Porous Barium Titanate Thin Film and Thermal Stabilization of Ferroelectric Phase by Porosity-Induced Strain

11.0K Views

article

10:40

A Fabrication and Measurement Method for a Flexible Ferroelectric Element Based on Van Der Waals Heteroepitaxy

8.2K Views

article

14:16

Fabrication of Schottky Diodes on Zn-polar BeMgZnO/ZnO Heterostructure Grown by Plasma-assisted Molecular Beam Epitaxy

7.6K Views

article

06:57

Theoretical Calculation and Experimental Verification for Dislocation Reduction in Germanium Epitaxial Layers with Semicylindrical Voids on Silicon

2.2K Views

article

11:34

Epitaxial Nanostructured α-Quartz Films on Silicon: From the Material to New Devices

5.4K Views

article

06:44

Tuning Oxide Properties by Oxygen Vacancy Control During Growth and Annealing

3.1K Views

JoVE Logo

Privacy

Terms of Use

Policies

Research

Education

ABOUT JoVE

Copyright © 2025 MyJoVE Corporation. All rights reserved